HP Compact Reactors (25-600 ml) HPCR-5500 Series

  • LEHPCR-5500 compact high pressure reactors cover 25-600 ml and use the vessel designs of the Micro and Mini Reactor families. The construction makes several changes to reduce the space occupied by the complete assembly:

    • A smaller magnetic drive takes the place of the larger drive assembly.
    • A compact variable speed motor drives the stirrer.
    • The larger support stand, overarm and motor are omitted.
    • An Aluminum Block Heater also acts as the reactor support.

    This arrangement suits laboratories with restricted space and users who do not need the full range of options or expansion possibilities of the larger stirred reactor family. It also supports multiple reactor installations for combinatorial chemistry and high throughput investigations.

    The reaction vessels are the same as those used in the Micro and Mini Reactor families and retain their split ring closure. Maximum working pressure is 2900 psi (200 bar). Temperature capability depends on the seal: a PTFE gasket permits operation to 350 °C, an FKM O-ring to 225 °C, and an FFKM O-ring to 275 °C.

    The 25, 50, and 100 mL sizes include an internal stirrer, gas inlet and outlet valves, a liquid sampling valve, a pressure gage, a safety rupture disc and an internal thermocouple. In addition to these fittings, the 300, 450, and 600 mL sizes can accept an optional internal cooling loop.

    Type 316 Stainless Steel is the standard vessel material. Any of the standard materials of construction can also be selected for this compact reactor family.

    Design to the ASME Pressure Vessel Code, European PED or other applicable local codes is available on request. Electrical safety requirements associated with CSA and CE are addressed on request.

    This description defines the product family. Guaranteed performance, included hardware, exclusions, interfaces and acceptance criteria are stated only in the project-specific technical proposal and approved datasheet.

    • HP Compact Reactors (25-600 ml) HPCR-5500 Series
    • HP Compact Reactors (25-600 ml) HPCR-5500 Series
    • HP Compact Reactors (25-600 ml) HPCR-5500 Series
  • Operating specifications

    • Compact high pressure reactor configuration.
    • Support arrangement: bench top.
    • Mounting arrangement: moveable vessel.
    • Available capacities, mL: 25mL to 600mL.
    • Standard maximum allowable working pressure, psi (bar): 2900 (200).
    • Operating temperature limits, ºC: 225 with FKM O-ring, 275 with FFKM O-ring and 350 with PTFE flat gasket.

    Magnetically coupled stirring

    A compact magnetic stirrer drive is configured specifically for the smaller reaction vessels. Its coupling uses compact magnet technology to transmit stirring motion into the vessel.

    Adjustable stirring speed

    A variable speed motor rated at 1/17 hp provides adjustment from 0 to 1700 rpm. An optional tachometer pickup sends its speed signal to an optional tachometer display module. This display module can be installed in the reactor temperature controller.

    Combined heater and vessel support

    The compact high pressure laboratory reactor uses a heater that also supports the vessel. An aluminum heating block distributes heat evenly around the reactor. The cartridge heating elements in the block can be replaced easily when needed. A stainless steel shield surrounds the heating block.

    Combining the heater and reactor support in this way reduces the footprint of the assembly. The arrangement occupies little bench space and suits installations where the available laboratory bench area is limited.

    Reactor temperature controller

    The reactor is supplied with the same type of temperature controller used for the standard medium and high pressure reactor range. Controller options include a redundant temperature sensor with alarm, a digital pressure reading, stirring speed indication or control, motor load monitoring and bi-directional digital communication through RS-485.

    Alternative process control

    A process controller is available as an alternative. A single process controller can operate up to eight compact high pressure laboratory reactors.

    Equipment options

    The ordering guide lists the configuration options for these compact reactors. Alongside the options described here, accessories include glass liners, PTFE liners, special stirrers, pressure gages, gas feed systems, liquid feed systems and custom valves. Additional accessories can be selected according to the application.

    The compact arrangement provides the basic functions required of a small laboratory reactor. Its packaging cannot accommodate every option available for the broader laboratory reactor range. Applications requiring explosion proof operation, jacketed vessels, bottom drain valves, high torque stirrers or catalyst baskets should use a micro reactor or mini reactor configuration as the starting point.

    Moveable vessel configuration25 mL50 mL100 mL, 1.3 x 4.5 inches300 mL450 mL600 mL160 mL100 mL, 2.0 x 2.0 inches
    Nominal internal volume, mL2550100300450600160100
    Maximum allowable working pressure (MAWP)2900 psi (200 bar)
    Operating temperature limits
    FKM O-ring seal225 °C
    FFKM O-ring seal275 °C
    PTFE flat gasket seal350 °C
    Reactor construction and equipment
    Vessel mounting arrangementMoveable
    Support arrangementCompact bench top
    Closure arrangementSplit-ring closure: 6 compression bolts with the flat gasket;
    no compression bolts with the O-ring seal.
    Valve connection threads1/8″ Male NPT
    Torque limit2.5 Inch-Pounds (0.28 Nm)
    Impeller quantity and diameter, 4 blades1 (0.81″ dia.)1 (0.81″ dia.)2 (1.38″ dia.)1 (0.81″ dia.)
    Stirring motor power1/17 hp
    Pressure gage diameter3.5 inches
    Pressure indication range0-3000 psi (207 bar)
    Temperature sensing arrangementFixed thermocouple
    Cooling coil provisionColdfinger, optionalStandard single loopSpiral, optional
    Bottom drain valve (BDV) provisionN/A
    Heating arrangementAluminum block, optional external cooling
    Heating power, Watts70010007001000700
    Electrical service requirements
    Supply voltage, Volts, AC115 / 230
    Maximum current, amps, 115 / 2308 / 410 / 58 / 410 / 58 /4
    Cylinder measurements
    Internal diameter x depth, inches1.0 x 2.01.3 x 2.251.3 x 4.52.5 x 4.02.5 x 6.02.5 x 8.02.5 x 2.02.0 x 2.0
    Assembled vessel weight, pounds1717181718201616
    Cylinder-only weight, pounds3.53.14.23.74.96.22.43.3
    Reactor and support measurements
    Width x depth excluding controller, inches8.3 x 9.5
    Overall height, inches2323252325272323
    Overall weight, pounds2525252628302525
    Replacement parts setSpare parts kit
  • Options and accessories allow reactors and pressure vessels to be configured for the reaction process and its intended operating conditions. The available equipment categories are listed below. They cover sample handling, catalyst work, heating, cooling, fluid transfer, stirring, measurement and vessel fittings.

    • Automatic liquid sampling equipment
    • Devices for adding catalyst
    • Baskets for catalyst containment
    • Toolkit for loading catalysts
    • System for catalyst testing
    • Condensation units
    • Pressure fittings with coned connections
    • Continuous feeder for bulk solids
    • Control equipment
    • Coils for vessel cooling
    • Equipment for operation in potentially ignitable atmospheres
    • Externally mounted valves and fittings
    • Systems for measuring gas
    • Gas measurement: intermediate supply tanks
    • Gas measurement: mass flow
    • Gas measurement: high pressure gas burettes
    • Vessel heating equipment
    • Electrical glands with insulation
    • Internal vessel liners
    • Systems for charging liquids
    • Liquid charging: metering pumps
    • Liquid charging: charging pipettes
    • Magnetically coupled drives
    • Drive assemblies and motors
    • Gages for pressure measurement
    • Hose for pressure service
    • Rupture discs for safety protection
    • Vessel for sample collection
    • Fixtures for servicing equipment
    • Devices for adding solids or slurry
    • Kits of replacement parts
    • Closures using split rings
    • Optional stirring arrangements
    • Impellers for gas entrainment
    • Operating temperature limits
    • Thermocouple sensors
    • Valve and fitting selections
    • Drain valves at the vessel bottom
    • Manual control valves for compressed gas tanks
    • Valves for pressure relief
    • Check valves for safety service
    • Viewing windows
  • The standard construction material for reactors is Type 316 Stainless Steel. Other alloys are also available. Reactors can be built from the following materials:

    • Type 316/316L Stainless Steel
    • Alloy A-286
    • Alloy 20
    • Alloy 230
    • Alloy 400
    • Alloy 600
    • Alloy 625
    • Alloy B-2/B-3
    • Alloy C-276
    • Nickel 200
    • Titanium Grades 2, 3, 4 and 7
    • Zirconium 702 and 705

    If a special alloy is specified for a reactor, the head, the cylinder and every internal wetted part of the vessel are made from that alloy. The external valves and fittings remain stainless steel. External parts are normally not exposed to the corrosive conditions present inside the vessel, so the extra cost of making them from special alloys is rarely justified.

    Alloy Designation

    The corrosion resistant alloys available for reactors and pressure vessels are identified here by alloy designation numbers. The same alloys are also known by trade names and by ASTM, ASME, DIN and other specification numbers. Many high nickel alloys were first patented and sold under trade names such as Monel, Inconel, Incoloy, Carpenter Alloy 20 and Hastelloy. Most of those patents have now expired. These alloys are now supplied as construction materials by other reputable producers as well as by the owners of the original trade names.

    Among the many corrosion resistant alloys on the market, two or three may have very similar compositions and serve the same corrosive environment. Each alloy still has its own physical strength, its own temperature characteristics and its own particular resistance to certain corrosive media. All of these factors have to be weighed when an alloy is selected, and cost and availability also influence the final choice.

    • MONEL, INCONEL and INCOLOY are registered trademarks of Special Metals Corp.
    • CARPENTER 20 is a registered trademark of Carpenter Technology Corporation.
    • HASTELLOY is a registered trademark of Haynes International, Inc.

    The table below gives the basic composition of these alloys. Data on corrosion resistance is available in corrosion handbooks and metallurgical publications. The individual alloy producers are also a useful source of information.

    Any short listing of the corrosion resistance of metals and alloys can mislead, because it cannot cover every effect of concentration, temperature, pressure and the presence of additional ions. Each of these has a significant effect on how well a reactor withstands corrosion. The susceptibility of a material to stress corrosion cracking, intergranular corrosion and pitting must also be taken into account when judging whether the material suits a particular application.

    The main characteristics of the construction materials offered are summarized below. These summaries are only a starting point for any study of comparative corrosion resistance and physical properties. Booklets from the material manufacturers on each alloy are available on request. Further details can also be found in other sources.

    Nominal Chemical Composition of Pressure Vessel Materials
    Major Elements (Percent)
    MaterialTypical Trade NameFeNiCrMoMnOther
    T316 Stainless Steel6512172.52.0Si 1.0
    Alloy 20Carpenter 203534202.52.0Cu 3.5, Cb 1.0 max
    Alloy 230Haynes 2303522220.7Co-5, W-14, Si-0.5
    Alloy 400Monel 4002.5 max63 min2 maxCu 31.5
    Alloy 600Inconel 60087615.5
    Alloy 625 Gr1Inconel 625 Gr15582290.5Cb+Ta 3.7
    Alloy A-286Alloy 2865325151.22Si-1, Ti-2.1, Al-0.35
    Alloy B-2/B-3Hastelloy B-2/B-32661281Co 1.0
    Alloy C-276Hastelloy C-2766.55315.5161W4.0, Co 2.5
    Nickel 20099
    Titanium Grade 2, 3, 4Commercially pure titaniumTi 99 min
    Titanium Grade 7Ti 98.8 min, 0.15 Pd
    Zirconium Grade 702Zr + Hf 99.2 min, Hf 4.5 max
    Zirconium Grade 705Zr + Hf 95.5 min, Hf 4.5 max, Nb 2.5

    Type 316/316L Stainless Steel

    Type 316 Stainless Steel performs very well with most organic systems. Under certain conditions a few organic acids and organic halides can hydrolyze and form inorganic halogen acids, and these attack T316SS. Acetic acid, formic acid and other organic acids are handled in T316SS as a matter of routine.

    T316SS is not usually the preferred material for inorganic acid systems. At ambient temperature it gives useful resistance to dilute sulfuric, sulfurous, phosphoric and nitric acids. At elevated temperature and pressure, however, sulfuric, phosphoric and nitric acids attack T316SS readily. Halogen acids attack every form of stainless steel quickly, even in dilute solutions and at low temperature.

    T316SS resists surface corrosion by caustics very well, but caustics can cause stress corrosion cracking in stainless pressure vessels. This effect starts to appear just above 100 °C and has been the most frequent cause of corrosion failure in stainless laboratory vessels. T316SS resists ammonia and most ammonia compounds well.

    Halogen salts can cause severe pitting in every stainless steel. Chlorides can cause stress corrosion cracking. Many other salt solutions, especially neutral or alkaline salts, can be handled in stainless vessels.

    At moderate temperature and pressure, T316SS is suitable for most commercial gases. In strictly anhydrous systems, even hydrogen chloride, hydrogen fluoride and chlorine can be handled in stainless steel.

    Practically all T316SS produced today also meets the specifications for T316L, the low carbon grade of stainless steel.

    Alloy 20

    Alloy 20 is an enriched stainless steel grade developed specifically for dilute sulfuric acid (up to 30 percent by weight) at elevated temperatures. It also suits nitric and phosphoric acid systems, as well as every system for which T316SS is suitable.

    Alloy 400

    Alloy 400 consists essentially of two-thirds nickel and one-third copper. In many applications its corrosion resistance is about equal to that of nickel. It allows higher maximum working pressures and temperatures and costs less, because it is much easier to machine.

    Alloy 400 is widely used with caustic solutions, since in most applications it does not suffer stress corrosion cracking. Chloride salts do not cause stress corrosion cracking in Alloy 400 either. It is also a very good material for fluorine, hydrogen fluoride and hydrofluoric acid systems. Alloy 400 has some resistance to hydrochloric and sulfuric acids at moderate temperatures and concentrations, but it is rarely the first choice for these acids. As its high copper content suggests, nitric acid and ammonia systems attack Alloy 400 rapidly.

    Alloy 600

    Alloy 600 is a high nickel alloy. It resists caustics and chlorides very well at high temperature and high pressure when sulfur compounds are present. In caustic environments no alloy performs better than Alloy 600. It is also often selected for its high strength at elevated temperatures. It can be recommended for a wide range of corrosive conditions, but its cost usually restricts its use to applications that need its exceptional properties.

    Alloy B-2/B-3

    Alloy B-2/B-3 is rich in nickel and molybdenum and was developed mainly to resist reducing acid environments, especially hydrochloric, sulfuric and phosphoric acids. In their pure forms it resists these acids better than any other alloy. Ferric ions and other oxidizing ions, even at levels as low as 50 ppm, can sharply reduce the resistance of this alloy.

    Alloy C-276

    Alloy C-276 is a nickel chromium-molybdenum alloy that probably has the widest general corrosion resistance of all commonly used alloys. It was first developed for wet chlorine service. It also resists strong oxidizers such as cupric and ferric chlorides very well, as well as many chlorine compounds and materials contaminated with chlorine. Thanks to this wide chemical resistance, Alloy C-276 is the second most widely used alloy after T316SS for research and development vessels.

    Nickel 200

    Nickel 200 is one designation of commercially pure nickel. It gives the highest corrosion resistance in hot caustic environments. Its use is strongly limited, however, by poor machinability and the high fabrication cost that follows from it.

    Titanium

    Titanium performs very well with oxidizing agents such as nitric acid, aqua regia and other mixed acids. It also resists chloride ions very well. Reducing acids such as sulfuric and hydrochloric acid corrode titanium at unacceptably high rates in pure form. These rates can drop to acceptable levels when relatively small amounts of oxidizing ions, such as cupric, ferric or nickel ions, or even nitric acid, are present and act as corrosion inhibitors.

    This effect has led to many successful uses of titanium in hydrometallurgy, where acids, especially sulfuric acid, are used to leach ores. In these processes the extracted ions act as corrosion inhibitors.

    Users must keep in mind that titanium burns vigorously in oxygen at elevated temperatures and pressures. Many hydrometallurgy applications handle oxygen and sulfuric acid successfully in titanium equipment, but the risk of ignition is always present. Protection against it is required whenever titanium and oxygen are used together.

    Commercially pure titanium comes in several grades. Grade 2 is the grade most often used for industrial equipment, because it can be welded. Vessels in Grade 2 can be built to the PED and ASME Codes on request. Grade 4 has slightly higher trace levels of iron and oxygen and is stronger than Grade 2. Grade 4 cannot be welded and is outside the PED and ASME Codes, so code design on request applies to Grade 2 only.

    Most vessels are not welded, so Grade 4 can give higher working pressures than Grade 2. Grade 7 contains small amounts of palladium. It gives improved resistance in certain environments and can be used for reactors and pressure vessels when suitable billets are available.

    Zirconium

    Zirconium resists hydrochloric and sulfuric acids very well. As with Alloy B-2/B-3, oxidizing ions such as ferric and cupric ions and fluorides must be avoided. Zirconium also resists phosphoric and nitric acids and alkaline solutions well. Two grades are available. Grade 702 contains hafnium and is the standard commercial grade, with the best resistance to most corrosive agents. Grade 705 contains small amounts of both hafnium and niobium. These additions raise its strength and permit higher maximum working pressures for a vessel. Grade 702 usually resists corrosion better than Grade 705, and Grade 702 is also easier to obtain from commercial raw material stocks.

    High Temperature / High Strength Alloys

    Besides the metals selected for corrosion resistance, some alloys are offered for their outstanding strength, their strength at high temperature, or both.

    Alloy 230

    Alloy 230 is listed among the alloys approved in ASME Section II for pressure vessel design. It is high in nickel, chromium, tungsten and cobalt. Its resistance is similar to that of Alloy 600, but it is normally chosen for its high strength at very high temperatures. It is sometimes chosen as a bolting material.

    Alloy 625

    Alloy 625 has chemical resistance similar to Alloy C-276, but is much stronger. It is used to obtain higher pressure ratings in high temperature applications.

    Alloy A-286

    Alloy A-286 belongs to the stainless steel family and keeps very high strength up to 371 °C. It is widely used as a bolting material.

    Pressure and Temperature Limits

    The maximum pressure and temperature for any reactor or pressure vessel depend on the vessel design, its construction material and the other components that form part of the design. Every material loses strength as temperature rises, so a pressure rating is only meaningful together with the temperature at which it applies. The ratings in the specification tables give the maximum allowable working pressure (MAWP) of each vessel in pounds per square inch (psi) and in bar, at the maximum rated temperature of that design, for a vessel made of Type 316 Stainless Steel. For vessels made of other alloys, the maximum pressure and temperature limits are calculated and assigned by engineering in line with all applicable regulations.

    A lower operating temperature can sometimes allow a higher working pressure. For example, the high temperature (HT) version of one reactor series is rated at 2000 psi (138 bar) maximum pressure and 500 °C maximum temperature. The standard version of the same series is rated at 2900 psi (200 bar) maximum pressure at 350 °C maximum temperature.

    It must not be assumed that a vessel operated at a lower temperature can be used above its rated MAWP. The rating may be governed by factors other than the strength of the vessel wall. The closure design, the magnetic drive, the seal type, the other components selected and the construction material can all limit the pressure and temperature ratings.

    As the table below shows, the maximum operating temperature of some materials is much lower than the value allowed for stainless steel.

    Maximum Allowable Temperatures
    Materials of ConstructionMaximum Temperature
    T316/316L Stainless Steelon request
    Alloy 20426 °C
    Alloy 230on request
    Alloy 400482 °C
    Alloy 600on request
    Alloy 625 Gr 1648 °C
    Alloy A-286371 °C
    Alloy B-2/B-3426 °C
    Alloy C-276on request
    Nickel 200315 °C
    Titanium Grade 2, 3, 4 and 7315 °C
    Zirconium Grade 702 and 705371 °C

    Safe calculation of the maximum working pressures and temperatures of reactors and pressure vessels involves multiple factors.