✓ In-house manufacturing — Hastelloy C276 & titanium✓ Custom engineering & prototypes✓ API / ASTM · CSA · CRN · CE✓ Serving US, Canada, EU, Middle East, Central Asia, Africa & LatAm

High Pressure/High Temperature Pressure Vessels (25-75 ml) HP/HTPV-4740 Series

  • LEHP/HTPV-4740 high pressure/high temperature vessels have a 1-inch bore and capacities of 25 or 75 mL. An alloy steel screw cap closes each vessel. Six cap screws apply the sealing load to a flat flexible graphite gasket.

    Interchangeable PTFE gaskets serve applications requiring high pressure but temperatures no higher than 350 °C. Above 350 °C, the allowable pressure decreases rapidly, reaching 1850 psi (125 bar) at 538 °C. All standard materials of construction are available, although the chosen material may reduce the permitted pressure and temperature.

    Only one opening can be accommodated in the head. It accepts a Gage Block Assembly, available with or without a thermocouple. A bench top ceramic fiber heater is offered only for the 75 mL vessel. The smaller 25 mL vessel is normally heated using an oven, bath, furnace or another general purpose heater.

    This description defines the product family. Guaranteed performance, included hardware, exclusions, interfaces and acceptance criteria are stated only in the project-specific technical proposal and approved datasheet.

    • High Pressure/High Temperature Pressure Vessels (25-75 ml) HP/HTPV-4740 Series
    • High Pressure/High Temperature Pressure Vessels (25-75 ml) HP/HTPV-4740 Series
    • High Pressure/High Temperature Pressure Vessels (25-75 ml) HP/HTPV-4740 Series
  • Basic Head and Pressure Relief Device

    Many non-stirred vessels offer a basic head with a plugged 1/8″ NPT port. This configuration is a starting point for a custom assembly because no safety relief device is fitted. The 1/8″ NPT plug leaves a connection where the user can install appropriate pressure relief equipment. Safety codes and accepted operating practice require adequate relief protection for every vessel.

    If a vessel is received without an installed safety relief device, the user must take responsibility for supplying and fitting that protection. The required protective device must be installed before the vessel enters service.

    Vessel FamilySmall high pressure and high temperature vessels
    Approximate Volume, mL2575
    Maximum Pressure (MAWP)
    Standard screw cap arrangement8500 psi (586 bar) @ 350 °C
    4100 psi (282 bar) @ 500 °C
    1850 psi (127 bar) @ 538 °C
    Alloy C-276 screw cap arrangement8500 psi (586 bar) @ 350 °C
    8000 psi (551 bar) @ 500 °C
    7900 psi (544 bar) @ 538 °C
    Maximum Temperature by Gasket
    Flat PTFE gasket350 °C
    Flat flexible graphite gasket500-538 °C
    Vessel Construction and Connections
    Head mounting arrangementMoveable
    Closure arrangementScrew cap fitted with 6 compression bolts
    Head sealing arrangementFlat gasket
    Head port arrangementsOne opening: “A” socket or a rupture disc assembly port
    Custom head port configurations are available on request after review of the required connection
    Maximum number of head openings1
    Optional temperature measurementThermocouple installed in the cylinder bottom or in an optional gage block assembly
    Optional Stand and Heating Equipment
    Stand arrangementN/ABench top stand with heater
    Heater constructionN/ACeramic fiber
    Heater power, WattsN/A700
    Maximum current load, amps, 115 V / 230 VN/A6 / 3
    Dimensions and Weights
    Cylinder internal diameter x depth, inches1.0 x 1.71.0 x 5.6
    Complete vessel weight, pounds*46
    Cylinder weight, pounds1.43.2
    *Weights apply to a moveable head vessel with its “A” socket plugged. The chosen head configuration and fittings affect the final vessel weight.
  • The standard construction material for reactors is Type 316 Stainless Steel. Other alloys are also available. Reactors can be built from the following materials:

    • Type 316/316L Stainless Steel
    • Alloy A-286
    • Alloy 20
    • Alloy 230
    • Alloy 400
    • Alloy 600
    • Alloy 625
    • Alloy B-2/B-3
    • Alloy C-276
    • Nickel 200
    • Titanium Grades 2, 3, 4 and 7
    • Zirconium 702 and 705

    If a special alloy is specified for a reactor, the head, the cylinder and every internal wetted part of the vessel are made from that alloy. The external valves and fittings remain stainless steel. External parts are normally not exposed to the corrosive conditions present inside the vessel, so the extra cost of making them from special alloys is rarely justified.

    Alloy Designation

    The corrosion resistant alloys available for reactors and pressure vessels are identified here by alloy designation numbers. The same alloys are also known by trade names and by ASTM, ASME, DIN and other specification numbers. Many high nickel alloys were first patented and sold under trade names such as Monel, Inconel, Incoloy, Carpenter Alloy 20 and Hastelloy. Most of those patents have now expired. These alloys are now supplied as construction materials by other reputable producers as well as by the owners of the original trade names.

    Among the many corrosion resistant alloys on the market, two or three may have very similar compositions and serve the same corrosive environment. Each alloy still has its own physical strength, its own temperature characteristics and its own particular resistance to certain corrosive media. All of these factors have to be weighed when an alloy is selected, and cost and availability also influence the final choice.

    • MONEL, INCONEL and INCOLOY are registered trademarks of Special Metals Corp.
    • CARPENTER 20 is a registered trademark of Carpenter Technology Corporation.
    • HASTELLOY is a registered trademark of Haynes International, Inc.

    The table below gives the basic composition of these alloys. Data on corrosion resistance is available in corrosion handbooks and metallurgical publications. The individual alloy producers are also a useful source of information.

    Any short listing of the corrosion resistance of metals and alloys can mislead, because it cannot cover every effect of concentration, temperature, pressure and the presence of additional ions. Each of these has a significant effect on how well a reactor withstands corrosion. The susceptibility of a material to stress corrosion cracking, intergranular corrosion and pitting must also be taken into account when judging whether the material suits a particular application.

    The main characteristics of the construction materials offered are summarized below. These summaries are only a starting point for any study of comparative corrosion resistance and physical properties. Booklets from the material manufacturers on each alloy are available on request. Further details can also be found in other sources.

    Nominal Chemical Composition of Pressure Vessel Materials
    Major Elements (Percent)
    MaterialTypical Trade NameFeNiCrMoMnOther
    T316 Stainless Steel6512172.52.0Si 1.0
    Alloy 20Carpenter 203534202.52.0Cu 3.5, Cb 1.0 max
    Alloy 230Haynes 2303522220.7Co-5, W-14, Si-0.5
    Alloy 400Monel 4002.5 max63 min2 maxCu 31.5
    Alloy 600Inconel 60087615.5
    Alloy 625 Gr1Inconel 625 Gr15582290.5Cb+Ta 3.7
    Alloy A-286Alloy 2865325151.22Si-1, Ti-2.1, Al-0.35
    Alloy B-2/B-3Hastelloy B-2/B-32661281Co 1.0
    Alloy C-276Hastelloy C-2766.55315.5161W4.0, Co 2.5
    Nickel 20099
    Titanium Grade 2, 3, 4Commercially pure titaniumTi 99 min
    Titanium Grade 7Ti 98.8 min, 0.15 Pd
    Zirconium Grade 702Zr + Hf 99.2 min, Hf 4.5 max
    Zirconium Grade 705Zr + Hf 95.5 min, Hf 4.5 max, Nb 2.5

    Type 316/316L Stainless Steel

    Type 316 Stainless Steel performs very well with most organic systems. Under certain conditions a few organic acids and organic halides can hydrolyze and form inorganic halogen acids, and these attack T316SS. Acetic acid, formic acid and other organic acids are handled in T316SS as a matter of routine.

    T316SS is not usually the preferred material for inorganic acid systems. At ambient temperature it gives useful resistance to dilute sulfuric, sulfurous, phosphoric and nitric acids. At elevated temperature and pressure, however, sulfuric, phosphoric and nitric acids attack T316SS readily. Halogen acids attack every form of stainless steel quickly, even in dilute solutions and at low temperature.

    T316SS resists surface corrosion by caustics very well, but caustics can cause stress corrosion cracking in stainless pressure vessels. This effect starts to appear just above 100 °C and has been the most frequent cause of corrosion failure in stainless laboratory vessels. T316SS resists ammonia and most ammonia compounds well.

    Halogen salts can cause severe pitting in every stainless steel. Chlorides can cause stress corrosion cracking. Many other salt solutions, especially neutral or alkaline salts, can be handled in stainless vessels.

    At moderate temperature and pressure, T316SS is suitable for most commercial gases. In strictly anhydrous systems, even hydrogen chloride, hydrogen fluoride and chlorine can be handled in stainless steel.

    Practically all T316SS produced today also meets the specifications for T316L, the low carbon grade of stainless steel.

    Alloy 20

    Alloy 20 is an enriched stainless steel grade developed specifically for dilute sulfuric acid (up to 30 percent by weight) at elevated temperatures. It also suits nitric and phosphoric acid systems, as well as every system for which T316SS is suitable.

    Alloy 400

    Alloy 400 consists essentially of two-thirds nickel and one-third copper. In many applications its corrosion resistance is about equal to that of nickel. It allows higher maximum working pressures and temperatures and costs less, because it is much easier to machine.

    Alloy 400 is widely used with caustic solutions, since in most applications it does not suffer stress corrosion cracking. Chloride salts do not cause stress corrosion cracking in Alloy 400 either. It is also a very good material for fluorine, hydrogen fluoride and hydrofluoric acid systems. Alloy 400 has some resistance to hydrochloric and sulfuric acids at moderate temperatures and concentrations, but it is rarely the first choice for these acids. As its high copper content suggests, nitric acid and ammonia systems attack Alloy 400 rapidly.

    Alloy 600

    Alloy 600 is a high nickel alloy. It resists caustics and chlorides very well at high temperature and high pressure when sulfur compounds are present. In caustic environments no alloy performs better than Alloy 600. It is also often selected for its high strength at elevated temperatures. It can be recommended for a wide range of corrosive conditions, but its cost usually restricts its use to applications that need its exceptional properties.

    Alloy B-2/B-3

    Alloy B-2/B-3 is rich in nickel and molybdenum and was developed mainly to resist reducing acid environments, especially hydrochloric, sulfuric and phosphoric acids. In their pure forms it resists these acids better than any other alloy. Ferric ions and other oxidizing ions, even at levels as low as 50 ppm, can sharply reduce the resistance of this alloy.

    Alloy C-276

    Alloy C-276 is a nickel chromium-molybdenum alloy that probably has the widest general corrosion resistance of all commonly used alloys. It was first developed for wet chlorine service. It also resists strong oxidizers such as cupric and ferric chlorides very well, as well as many chlorine compounds and materials contaminated with chlorine. Thanks to this wide chemical resistance, Alloy C-276 is the second most widely used alloy after T316SS for research and development vessels.

    Nickel 200

    Nickel 200 is one designation of commercially pure nickel. It gives the highest corrosion resistance in hot caustic environments. Its use is strongly limited, however, by poor machinability and the high fabrication cost that follows from it.

    Titanium

    Titanium performs very well with oxidizing agents such as nitric acid, aqua regia and other mixed acids. It also resists chloride ions very well. Reducing acids such as sulfuric and hydrochloric acid corrode titanium at unacceptably high rates in pure form. These rates can drop to acceptable levels when relatively small amounts of oxidizing ions, such as cupric, ferric or nickel ions, or even nitric acid, are present and act as corrosion inhibitors.

    This effect has led to many successful uses of titanium in hydrometallurgy, where acids, especially sulfuric acid, are used to leach ores. In these processes the extracted ions act as corrosion inhibitors.

    Users must keep in mind that titanium burns vigorously in oxygen at elevated temperatures and pressures. Many hydrometallurgy applications handle oxygen and sulfuric acid successfully in titanium equipment, but the risk of ignition is always present. Protection against it is required whenever titanium and oxygen are used together.

    Commercially pure titanium comes in several grades. Grade 2 is the grade most often used for industrial equipment, because it can be welded. Vessels in Grade 2 can be built to the PED and ASME Codes on request. Grade 4 has slightly higher trace levels of iron and oxygen and is stronger than Grade 2. Grade 4 cannot be welded and is outside the PED and ASME Codes, so code design on request applies to Grade 2 only.

    Most vessels are not welded, so Grade 4 can give higher working pressures than Grade 2. Grade 7 contains small amounts of palladium. It gives improved resistance in certain environments and can be used for reactors and pressure vessels when suitable billets are available.

    Zirconium

    Zirconium resists hydrochloric and sulfuric acids very well. As with Alloy B-2/B-3, oxidizing ions such as ferric and cupric ions and fluorides must be avoided. Zirconium also resists phosphoric and nitric acids and alkaline solutions well. Two grades are available. Grade 702 contains hafnium and is the standard commercial grade, with the best resistance to most corrosive agents. Grade 705 contains small amounts of both hafnium and niobium. These additions raise its strength and permit higher maximum working pressures for a vessel. Grade 702 usually resists corrosion better than Grade 705, and Grade 702 is also easier to obtain from commercial raw material stocks.

    High Temperature / High Strength Alloys

    Besides the metals selected for corrosion resistance, some alloys are offered for their outstanding strength, their strength at high temperature, or both.

    Alloy 230

    Alloy 230 is listed among the alloys approved in ASME Section II for pressure vessel design. It is high in nickel, chromium, tungsten and cobalt. Its resistance is similar to that of Alloy 600, but it is normally chosen for its high strength at very high temperatures. It is sometimes chosen as a bolting material.

    Alloy 625

    Alloy 625 has chemical resistance similar to Alloy C-276, but is much stronger. It is used to obtain higher pressure ratings in high temperature applications.

    Alloy A-286

    Alloy A-286 belongs to the stainless steel family and keeps very high strength up to 371 °C. It is widely used as a bolting material.

    Pressure and Temperature Limits

    The maximum pressure and temperature for any reactor or pressure vessel depend on the vessel design, its construction material and the other components that form part of the design. Every material loses strength as temperature rises, so a pressure rating is only meaningful together with the temperature at which it applies. The ratings in the specification tables give the maximum allowable working pressure (MAWP) of each vessel in pounds per square inch (psi) and in bar, at the maximum rated temperature of that design, for a vessel made of Type 316 Stainless Steel. For vessels made of other alloys, the maximum pressure and temperature limits are calculated and assigned by engineering in line with all applicable regulations.

    A lower operating temperature can sometimes allow a higher working pressure. For example, the high temperature (HT) version of one reactor series is rated at 2000 psi (138 bar) maximum pressure and 500 °C maximum temperature. The standard version of the same series is rated at 2900 psi (200 bar) maximum pressure at 350 °C maximum temperature.

    It must not be assumed that a vessel operated at a lower temperature can be used above its rated MAWP. The rating may be governed by factors other than the strength of the vessel wall. The closure design, the magnetic drive, the seal type, the other components selected and the construction material can all limit the pressure and temperature ratings.

    As the table below shows, the maximum operating temperature of some materials is much lower than the value allowed for stainless steel.

    Maximum Allowable Temperatures
    Materials of ConstructionMaximum Temperature
    T316/316L Stainless Steelon request
    Alloy 20426 °C
    Alloy 230on request
    Alloy 400482 °C
    Alloy 600on request
    Alloy 625 Gr 1648 °C
    Alloy A-286371 °C
    Alloy B-2/B-3426 °C
    Alloy C-276on request
    Nickel 200315 °C
    Titanium Grade 2, 3, 4 and 7315 °C
    Zirconium Grade 702 and 705371 °C

    Safe calculation of the maximum working pressures and temperatures of reactors and pressure vessels involves multiple factors.

  • Optional equipment and connection fittings allow a pressure vessel to be configured for its specified duty. The available accessories cover heating, temperature control, pressure measurement, connections and sample handling.

    Main Accessory Groups

    • Vessel heaters
    • Controllers for temperature regulation
    • Gage block assemblies for pressure measurement
    • Coned fittings for pressure connections
    • Valves and associated fittings

    Additional Accessories*

    • Automated sampling unit for liquids
    • Vessel liners
    • Hose for pressure service
    • Safety check valves
    • Pipettes for liquid addition
    • Systems for gas filling

    *Installing these accessories may require changes to the vessel.

  • Head Gaskets and Sealing Materials

    Reactor and pressure vessel heads can use four types of gasket material. Each type has a particular operating range, useful properties and restrictions. The available materials provide several ways to match the closure arrangement and the head seal to the intended process conditions. Selection must account for the temperature and chemical exposure as well as the way the closure applies force to the gasket.

    Fully Confined Flat PTFE Gaskets: Operation to 350 °C

    A flat gasket of PTFE fluoropolymer is the usual and most widely used head seal for these vessels. The cover contains a recessed seat for the gasket. When the cylinder lip enters this recess, it encloses the seal on all sides except for a narrow inner edge that contacts the vessel contents. Confinement of the gasket, together with the properties of PTFE, allows the closure to seal reliably at working temperatures up to 350 °C.

    The flat gasket needs an initial compressive load to establish a leak-tight joint and retain that joint during operation. A circle of cap screws in the split-ring cover clamp supplies this load. PTFE deforms slightly under pressure and flows against the sealing faces of the cylinder and head. Repeated use can therefore improve contact as the gasket conforms to those faces. This ability to deform also makes the seal less sensitive to small differences in loading. Metal gaskets and other materials that do not flow require greater care to distribute the load uniformly.

    A further reason to use PTFE is its resistance to an exceptionally wide range of chemicals. This broad chemical compatibility is a major part of its suitability as a main head gasket.

    O-Ring Closures That Seal Under Internal Pressure

    Self-sealing O-ring heads are available for a range of reactors and pressure vessels. Internal vessel pressure supplies the sealing force in this arrangement. The split-ring sections hold the cylinder and head together; they do not need cap screws to apply an initial compression load to the seal. This separates the mechanical locking function of the ring from the pressure-generated sealing action of the O-ring.

    Selection of an elastomeric O-ring requires attention to two limitations. Its allowable operating temperature is lower than that of a PTFE gasket, and its chemical resistance is less universal. Compatibility is particularly relevant because the O-ring contacts the process contents directly. Although several elastomers are available, the usual choices are FKM and FFKM. Fluoroelastomer (FKM) is commonly selected first for a self-sealing closure. It combines good chemical resistance with a working temperature up to 225 °C. Perfluoroelastomer (FFKM) provides a much wider range of chemical resistance and permits working temperatures up to 275 °C.

    FFKM is a specialty sealing material. Its 275 °C operating limit extends the range of elastomeric closures, but a flat PTFE gasket with a 350 °C limit is generally the more suitable choice when operation at that temperature level is planned. Other specialty O-ring materials can also be supplied. Ethylene-propylene is another option: it resists certain substances that attack FKM, with a modest reduction in allowable operating temperature. The final material choice therefore depends on both chemical exposure and the required temperature range.

    Confined Flat Flexible Graphite Gaskets: Operation to 600 °C

    Flexible graphite provides a head seal for operating temperatures above 350 °C. The gasket consists of bonded, flexible graphite layers. These layers form a seal almost as readily as flat PTFE while providing high temperature capability and strong chemical resistance. The material has a broad temperature range; the working limit of an assembled vessel remains dependent on its specified configuration.

    Standard high temperature arrangements accept flat flexible graphite gaskets in place of the metal seals previously used above 350 °C. The graphite gasket sits in the same type of groove as a PTFE gasket, and the closure uses the same split-ring arrangement. A PTFE gasket can consequently be substituted when the vessel will operate below 350 °C. Flexible graphite seals can be used again, although their service life is generally shorter than the service life of PTFE seals.

    Metal Head Gaskets

    Metal seals were historically the available choice for temperatures above 350 °C. A metal gasket with a diamond-shaped cross-section remains available for special duties. Flexible graphite is the preferred alternative for most applications in this temperature range, while the metal arrangement serves applications that specifically require it.

    Generic Names for Seal Materials

    Sealing materials are frequently identified by proprietary trade names rather than their material descriptions. The terminology below uses generic material names and abbreviations so that the seal can be specified by its composition. ASTM material designations are used where available. The table retains the separate common-name, material and designation fields for each sealing material.

    Generic Common NameMaterialDesignation
    Fluoroelastomer sealfluoroelastomerFKM
    Perfluoroelastomer sealperfluoroelastomerFFKM
    PTFE sealtetrafluoroethylene polymerPTFE
    Flexible graphite sealflexible graphiteFG
    • Proprietary names for fluoroelastomer, perfluoroelastomer and tetrafluoroethylene polymer are replaced here by the corresponding generic material terms.
    • The proprietary name for flexible graphite is replaced here by its generic material description.

    Pressure Measurement Gages

    Pressure vessel gages are available with 3-1/2 inch or 4-1/2 inch dials and the ranges listed below. Standard construction uses a stainless steel Bourdon tube and a 1/4 inch NPT male connection. Alloy 400 gages can be supplied on request. Accuracy of both gage sizes is 1 percent of full scale. Standard dials have two scales, graduated in pounds per square inch (psi) and bars. Pascal graduations are available on request. Compound gages cover vacuum to 30 inches of Mercury and positive pressure to 300 psi/20 bar.

    For a nonstandard gage, specify the required dial diameter, measuring range and scale units. These details determine the gage configuration for the vessel.

    Select a full-scale gage range equal to 150 percent of the maximum operating pressure. This places the working pressure in the more accurate part of the range. It also avoids repeatedly loading the gage to full scale, which can change its calibration over time.

    Pressure Range psiPressure Range bar4-1/2″ Diameter Gage3-1/2″ Diameter Gage3-1/2″ Diameter Back Mount Gage
    0-1000-7Pressure gagePressure gageBack mount pressure gage
    0-2000-14Pressure gagePressure gageBack mount pressure gage
    0-6000-40Pressure gagePressure gageBack mount pressure gage
    0-10000-70Pressure gagePressure gageBack mount pressure gage
    0-20000-140Pressure gagePressure gageBack mount pressure gage
    0-30000-210Pressure gagePressure gageBack mount pressure gage
    0-40000-280NAPressure gage-
    0-50000-350Pressure gagePressure gage-
    0-75000-517Pressure gageNA-
    0-100000-700Pressure gageNA-
    30″ Hg Vac/300 psiCompound gageCompound gageBack mount compound gage

    Rupture Discs for Pressure Protection

    Purpose-made rupture discs protect the pressure vessels. Each disc has a domed profile formed during manufacture by applying 70% of its burst pressure to that individual disc. The dome therefore results from the forming pressure applied to the disc before it enters service.

    Design to ASME or other pressure vessel codes is available on request. The rupture disc selection principle limits its burst pressure to no more than the vessel design pressure. For pressure loading without rapid cycling, the recommended operating limit is 90% of the disc burst pressure. Applied together, these limits restrict vessel operating pressure to no more than 90% of the vessel design pressure.

    Standard rupture discs use Alloy 600. This alloy offers high corrosion resistance and retains over 90% of its room temperature rating at temperatures up to 450 °C. Gold facing can increase corrosion resistance; alternatively, discs can be made from Alloy C276. A disc can be matched to the required working pressure and temperature above the stated minimum limits.

    Vessels and reactors from 25 mL to 2000 mL use Alloy 600 discs, with a gold-faced Alloy 600 version also available. Vessels of 1 gallon and larger use the larger-vessel disc arrangement. The Safety Rupture Disc Assemblies Operating Instructions provide the selection listing, burst ranges and material details for these assemblies.

    For Alloy 600 discs, the lowest general range for the small-vessel plain and gold-faced versions is 1000 psi. The larger-vessel version starts at 1000 psi, as shown in the table. Other disc materials can provide alternative ranges, but they do not retain the same combination of corrosion resistance and high temperature capability.

    Where a lower-range pressure gage is preferred, a spring-loaded relief valve can be set to protect that gage. A 1000 psi rupture disc then provides the fail-safe pressure protection. Special rupture disc requirements can be reviewed on request, including the required operating conditions and assembly arrangement.

    Discs for a 1/4″ Orifice
    Burst Rating, psigAlloy 600 DiscGold Faced Alloy 600 Disc
    1000Rupture discGold faced rupture disc
    2000Rupture discGold faced rupture disc
    3000Rupture discGold faced rupture disc
    4000Rupture discGold faced rupture disc
    5000Rupture discGold faced rupture disc
    8000Rupture discGold faced rupture disc
    10000Rupture disc-
    Discs for a 1/2″ Orifice
    Burst Rating, psigAlloy 600 Disc
    1000Larger-vessel rupture disc
    1500Larger-vessel rupture disc
    2000Larger-vessel rupture disc
    3000Larger-vessel rupture disc
Coretest